High BOROSILICATE3.3 GLASS
SiO2 Content | >80% |
Strain Point | 520ºC |
Annealing Point | 560ºC |
Softening Point | 820ºC |
Refractive Index | 1.47 |
Light Transnission(2mm) | 0.92 |
Elastic Modulus | 67KNmm-2 |
Tensile Strength | 40-120Nmm2 |
Glass Stress Optical Coefficient | 3.8*106m2/N |
Processing Temperature (104dpas) | 1220ºC |
Linear Coefficient of Expansion(20-300ºC) | 3.3*10-6K-1 |
Density(20ºC) | 2.23gcm-1 |
Specific Heat | 0.9jg-1K-1 |
Thermal Conductivity |